The invention discloses a preparation method of overlength Cu-Cr-Zr alloyed contact line. The smelting content in an induction furnace is Cu-(0.30-0.60) %Cr-(0.10-0.15) %Zr-(0.01-0.02) %Si alloy. By processes of continuous casting, extrusion, heat treatment, cold drawing and rolling, a contact line with a nominal area of 110-150mm is prepared, under the conditions that processes are simplified and equipment and alloying components are fairly simple, the contact line with a length of simple root of the finished product being up to 1000-1500m has fine tensile strength, electrical conductivity and high temperature softening resistance.