Time multiplexed deep reactive ion etching of germanium and silicon—A comparison of mechanisms and application to x-ray optics

2018 
Although the mechanisms of deep reactive ion etching (DRIE) of silicon have been reported extensively, very little by comparison has been discussed concerning DRIE of germanium. By directly comparing silicon and germanium etching in a time multiplexed DRIE process, the authors extract significant differences in etch mechanisms from a design of experiment and discuss how these differences are relevant to the design and fabrication of silicon and germanium collimating channel array x-ray optics. The differences are illuminated by characteristics such as reactive ion etching (RIE)-lag, aspect ratio dependent etching, and sidewall passivation. Specifically, the authors demonstrate the more severe nature of RIE-lag in germanium, especially at aspect ratios exceeding 13:1. In addition, the differences in the profile evolution between silicon and germanium are shown to be a result of differences in sidewall passivation. There is also a correlation between the different sidewall passivation and the inherent lack ...
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    14
    References
    0
    Citations
    NaN
    KQI
    []