Laminate and stretching the laminate using the same

2010 
TamaAkira径 polyglycolic acid resin 100 parts by weight of the crystallization of 1 to 30 [mu] m, and at least one nucleating agent boron nitride particles is selected from the group consisting of molybdenum disulfide particles and tungsten disulfide particles from 0.0075 to 0 laminate comprising .20 and crystallized polyglycolic acid-based resin layer containing the parts by weight, and a thermoplastic resin layer adjacent to the crystallization polyglycolic acid resin layer.