Compounds and method of preparing an aqueous asphalt emulsion storable cold mix formula

2014 
The present invention discloses a storable cold mix emulsion type aqueous asphalt mixture, the mass ratio as follows: stone 100, the charge control agent 2 ~ 4, an aqueous cold mix asphalt emulsion 5-6, emulsion diesel 0.2-0.4; mass charge control agent ratio: 2 to 4, sodium carbonate, sodium hydroxide 0.5 to 1, 95.5 to 97 water; emulsion mass ratio of diesel: diesel 70, water 30, TX-4 0.006; cold aqueous asphalt emulsion mix mass ratio: three yuan amphoteric surface active agent, an aqueous solution of 60 to 70, 30 to 40 and asphalt mixture aquasorb 0.03-0.04; three yuan aqueous mass ratio of amphoteric surfactant: amphoteric surfactant paste three yuan 2, water 98; paste three yuan amphoteric surfactants mass ratio of amphoteric surfactant ternary 50, water 50, wherein the amphoteric surfactant is a three yuan five kinds of lignin; asphalt mixture mass ratio: 93.5 to 94.5 bitumen, naphthenic oil 5 1-6, Carlo amine 0.5.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    0
    Citations
    NaN
    KQI
    []