Bioactive resorbed porous 3d-matrix for regenerative medicine and method for preparing it

2013 
FIELD: medicine. SUBSTANCE: bioactive porous 3D-matrix for tissue engineering involves a resorbed partially crystalline polymer having a porosity of 60-80% and a pore size of 2 to 100 mcm. A biopolymer gel having a particle size of 30-100 mcm is incorporated into a portion of the pores. A polymer/gel ratio makes 99:1 to 50:50 wt %. The matrix is prepared by grinding a mixture of gel and polymer powder having an average particle size of 100 mcm, and the prepared mixture fills prepared moulds to be placed in a high-pressure chamber wherein the temperature is increased to 25-40°C first, and then the CO 2 pressure is increased to 4.0-25.0 MPa. The system is kept in the above environment for 1 hour, and then the chamber pressure is discharged to an atmospheric one for 30-120 minutes; thereafter the temperature is decreased to a room value, and the patterns are removed. EFFECT: ensuring flexibility of using the matrix in various organs and systems, no toxicity, higher ability to tissue regeneration stimulation, prolonged effect of biostimulation. 6 cl, 5 ex, 1 tbl, 4 dwg
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    1
    References
    0
    Citations
    NaN
    KQI
    []