No-nickel flux-cored wire and preparation method and application thereof

2015 
The invention discloses a no-nickel flux-cored wire and a preparation method and application thereof. The no-nickel flux-cored wire consists of a carbon steel cover and medicine powder filled in the cover; the filling rate is 13.0-18.0%; the medicine powder comprises the following components in percentage by mass: 5.0-8.0% of TiO2, 0.6-1.5% of SiO2, 0.5-1.5% of ZrO2, 1.5-3.0% of Mn, 0.4-1.2% of Si, 0.20-0.60% of MgO, 0.10-0.50% of CaCO3, 0.10-0.20% of CaF2, 0.10-0.30% of NaF, 0.010-0.020% of Re, 0.40-0.70% of magnesium aluminum alloys, and the balance of Fe. The flux-cored wire has high toughness and excellent crack resistance, can be welded in all positions, and is specifically suitable for steel plates with yield strength equal to or higher than 390 MPa.