Overcharge and thermal destructive testing of lithium metal oxide and lithium metal phosphate batteries incorporating optical diagnostics

2017 
Abstract Lithium batteries have a tendency to fail violently under adverse conditions leading to the rapid venting of gas. Overcharge, thermal heating, and a combination of the two conditions are applied here to investigate the gas venting process. A test chamber has been constructed with data recordings including chamber pressure and temperature, battery voltage, current, and surface temperature as functions of time throughout the charging and failure processes. High-speed imaging and schlieren flow visualization are used to visualize the gas venting process. A direct comparison between lithium iron phosphate based K2 26650 and lithium nickel manganese cobalt oxide LG 18650 cells is made through a test series of the three failure methods. Failure under thermal, overcharge, and thermal-overcharge conditions are generally similar in terms of the gas venting process, but are observed to have increasingly energetic failures. The thermal-overcharge abuse condition demonstrates an ability to reconnect via internal short circuit even after an initial electrical failure seen as the refusal to accept charge. This reconnection is associated with a secondary, more energetic failure which can produce weak shock pressure waves.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    16
    References
    14
    Citations
    NaN
    KQI
    []