Study on prevention of welding defects in high power CO2 laser materials processing

1999 
For CO2 laser welding of large output, when a deep penetration welding in single pass is done in the ambient atmosphere, it is known that blowholes may occur because of the in-keyhole gas being entrapped in molten metal. Keeping this problem in mind and changing the parameters, we conducted welding tests with full-penetration bead-on-plate welding, and checked by radiographic test for welding defects. The experimental results demonstrated that the larger the specimen thickness, the more frequently welding defects occur, and that generation of welding defects depends upon the amount of welding heat input. Welding defects such as blowholes remain in metal, because the gas once entrapped into keyhole floats up in molten metal, and it is enclosed in the course of solidification. From this, we can verify the theory that a larger welding heat input, in the case of the good appearance full-penetration bead-on-plate welding, may be favorable for preventing welding blowholes. It can be assumed, therefore, that a l...
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    2
    Citations
    NaN
    KQI
    []