A thermoplastic molding material for automotive interior applications

1998 
The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    0
    Citations
    NaN
    KQI
    []