Formation of high-Tc Bi1.6Pb0.4Sr2Ca2(Cu0.9Ti0.1)3Ox

1993 
Influences of sintering conditions onTc are studied for Bi1.6Pb0.4Sr2Ca2(Cu0.9Ti0.1)3O x . HighTc values are obtained at 1123±5 K sintering temperature and over 50 h sintering time. In order to explain theTc changes, morphological discussion is attempted.