Interaction of a Nanosized Pd Catalyst with Active C from the Carbon Support: An Advanced in Situ XRD Study
2011
We have used in situ X-ray diffraction and line profile analysis to study the carburization of a 6 nm Pd catalyst supported on carbon at various temperatures under helium, hydrogen, and oxygen. A maximum of 10% C atoms was dissolved in the Pd lattice. This phase is stable at ambient conditions but decays above 400 °C. The rate of formation is limited by active C from the support and is slower by a factor of ∼100 compared to the supply of C atoms via CO decomposition. The bulk diffusion coefficient predicts an even faster rate, demanding a surface barrier to activate bulk diffusion. We find that the rate of formation depends on the surface to volume ratio. Carbon is nonuniformly distributed among individual Pd particles, but hydrogen fills interstitial sites to lift the irregularity. In the ternary phase PdCxHy, x and y are linearly linked. Oxygen reacts with interstitial carbon already below 160 °C.
Keywords:
- Correction
- Source
- Cite
- Save
- Machine Reading By IdeaReader
41
References
28
Citations
NaN
KQI