Thermal degradation of fluorotelomer treated articles and related materials

2005 
Abstract This study reports the first known studies to investigate the thermal degradation of a polyester/cellulose fabric substrate (“article”) treated with a fluorotelomer-based acrylic polymer under laboratory conditions conservatively representing typical combustion conditions of time, temperature, and excess air level in a municipal incinerator, with an average temperature of 1000 °C or greater over approximately 2 s residence time. The results demonstrate that the polyester/cellulose fabric treated with a fluorotelomer-based acrylic polymer is destroyed and no detectable amount of perfluorooctanoic acid (PFOA) is formed under typical municipal incineration conditions. Therefore, textiles and paper treated with such a fluorotelomer-based acrylic polymer disposed of in municipal waste and incinerated are expected to be destroyed and not be a significant source of PFOA in the environment.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    26
    References
    56
    Citations
    NaN
    KQI
    []