Non-Standard T6 Heat Treatment of the Casting of the Combustion Engine Cylinder Head

2020 
The introduction of new design solutions of cast components to the powertrain systems of passenger cars has resulted in an increased demand for optimization of mechanical properties obtained during heat treatment, assuring—at the same time—a suitable level of production capacity and limitation of manufacturing costs. In this paper, research results concerning non-standard T6 heat treatment of a combustion engine cylinder head made of AlSi7Cu3Mg alloy are presented. It has been confirmed that the optimal process of heat treatment of this component, taking into consideration the criterion of material hardness, involves solutioning at a temperature of 500 °C for 1 h, and then aging for 2 h at 175 °C. As a result, HBS10/1000/30 hardness in the range of 105–130 was obtained, which means an increase from 35% to 60% in comparison to the as-cast, depending on the position of the measurement and spheroidization of precipitations of eutectic silicon.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    2
    Citations
    NaN
    KQI
    []