Thermoplastic molding compositions based on styrene copolymers and polyamides having improved weatherability

2010 
Material thermoplastic molding, containing, a) from 3 to 78% by weight of one or more copolymers of styrene, which have no unit derived I deanhidrido maleic acid, as component A, b) 15 to 90 wt% one or more polyamides as component B, c) from 5 to 50% by weight of one or more graft rubbers which modify the impact strength without olefinic doblesenlaces in the rubber phase as component C, d) 1 to 25% weight of one or more copolymers of styrene, which, relative to the total component D, present from 0.5 to 5% by weight of units derived from maleic anhydride, as component D, e) 1 to 30% by weight one or more additional olefinic monomers based without estructuranucleo-wrapped and at least 0.1% by weight of functional monomers as component E, f) 0 to 50% by weight of one or more fillers in rubbers fiber form or in particle form comocomponente F, g) from 0 to 40% by pes or further additives as component G, resulting in the total amount of the components A to E and optionally F and G 100% by weight.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    0
    Citations
    NaN
    KQI
    []