Chain-folded lamellar structure and dynamics of the crystalline fraction of Bombyx mori silk fibroin and of (Ala-Gly-Ser-Gly-Ala-Gly)n model peptides.

2020 
Abstract Solid-state NMR is a powerful analytical technique to determine the composite structure of Bombyx mori silk fibroin (SF). In our previous paper, we proposed a lamellar structure for Ala-Gly copolypeptides as a model of the crystalline fraction in Silk II. In this paper, the structure and dynamics of the crystalline fraction and of a better mimic of the crystalline fraction, (Ala-Gly-Ser-Gly-Ala-Gly)n (n = 2–5, 8), and 13C selectively labeled [3-13C]Ala-(AGSGAG)5 in Silk II forms, were studied using structural and dynamical analyses of the Ala Cβ peaks in 13C cross polarization/ magic angle spinning NMR and 13C solid-state spin-lattice relaxation time (T1) measurements, respectively. Like Ala-Gly copolypeptides, these materials have lamellar structures with two kinds of Ala residues in β-sheet, A and B, plus one distorted β-turn, t, formed by repetitive folding using β-turns every eighth amino acid in an antipolar arrangement. However, because of the presence of Ser residues at every sixth residue in (AGSGAG)n, the T1 values and mobilities of B decreased significantly. We conclude that the Ser hydroxyls hydrogen bond to adjacent lamellar layers and fix them together in a similar way to Velcro®.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    47
    References
    4
    Citations
    NaN
    KQI
    []