Method for producing an electrochemical element electrode conductive adhesive composition

2014 
Conductive carbon, a first step of agitating the slurry containing the particulate binder and a dispersion medium at a temperature range of 5 to 40 ° C., the slurry was stirred at the first step, the process pressure 80~230Mpa, nozzle diameter and a second step of treating with a high-pressure dispersing machine 2 of 100 to 500 [mu] m.