Grain-size composition, shape and morphology study of titanium powder particles produced by electroerosion dispersion

2015 
This article describes the method of electroerosion dispersion, and study results for grain-size composition, shape and morphology of titanium particles produced in distilled water. It was established experimentally that the average particle size is 33.12 m, arithmetical value - 33.121 µm, specific surface area - 10151.91 cm2/sec3, elongation coefficient (extension) of particles with a size of 31.372 µm was 2.59. This article presents the microscopical investigation results for titanium powder samples.