Abstract Methane reforming in steam (SR), auto-thermal (ATR) and partial oxidation (POX) conditions over Ni/Ba–Ce 0.9 –Y 0.1 catalyst was investigated in the temperature range 500–700 °C. Catalyst presents a satisfying activity in POX condition only. BCY carrier was not stable in the presence of CO 2 and, irrespective of reaction conditions, it reacts with CO 2 giving rise to the formation of BaCO 3 and CeO 2 . The very low activity observed in SR conditions was due to the negative role exerted by water strongly absorbed on catalyst surface, limiting so the accessibility and reduction state of Ni active sites. In POX condition catalyst is active and satisfying H 2 yield can be reached by operating at T  = 700 °C. A significant reduction of coke formation was observed by operating in POX at 700 °C. On the contrary, in ATR condition at the same reaction temperature huge amount of filamentous coke was observed.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    13
    References
    8
    Citations
    NaN
    KQI
    []