Effect of biofilm formation, and biocorrosion on denture base fractures

2013 
Three different heat polymerized acrylic resins (Ivocap Plus, Lucitone 550, QC 20) were used to prepare three different types of samples. Type “A” samples with “V” type notch was used to measure the fracture strength, “B” type to evaluate the surfaces with scanning electron microscopy and “C” type for quantitative biofilm assay. Development and calculation of biofilm covered surfaces on denture base materials were accomplished by SEM and quantitative biofilm assay. According to normality assumptions ANOVA or Kruskal-Wallis was selected for statistical analysis (α=0.05).