Mechanical performance of metal-ceramic interfaces produced by laser processing

1995 
This paper concentrates on the mechanical performance of various ceramic coatings of Cr2O3 on steel (SAF2205), as produced by CO2 laser processing. The thickness of the coating that can be applied by laser coating is limited to about 200 μm setting a limit to the maximum strain energy release rate that can be measured in a 4 point flexure test before severe yielding occurs. In addition, a network of cracks with spacings of the order of 200 μm was always present in the laser applied coating preventing steady state crack growth along the interface.