Charge Storage Behavior of Nanowire Transistors Functionalized with Bis(terpyridine) -- Fe(II) Molecules: Dependence on Molecular Structure

2004 
We studied the influence of three bis(terpyridine)−Fe(II) molecules(X-tpy)2FeCl2 (X = H (1), SAc (2), and 4-phenyl-SAc (3)on charge storage of a nanowire transistor. The molecules were assembled on the surface of an indium oxide nanowire that forms the conduction channel of the transistor. We found that the charge storage characteristics of such a device strongly depends on the structure of the terpyridine ligand:  both retention time (τ) and threshold voltage shift (ΔVth) increased in the order of 1 < 2 < 3, with τ of 200 s, 12 h, and 287 h and ΔVth at 4.8, 12, and 28 V, respectively. Furthermore, when we placed the devices with molecules 1 and 3 in a vacuum and recorded the I−Vg curves in a two-day period, we observed higher hysteresis stability for device with molecule 3. For example, ΔVth was reduced from 4.8 to 1.7 V for the device with molecule 1, while there was no reduction in ΔVth for the device with molecule 2. These results suggest that thiolate headgroup and/or longer ligand length raises the ...
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    22
    References
    48
    Citations
    NaN
    KQI
    []