Intelligent energy shunting fluid/fabric base structure which utilizes well-processed shear thickening fluid has been developed. The shear thickening fluid has been synthesized by a powerful mechanical stirrer to disperse 12 nm silica particles into polyethylene glycol 200 g/mol at three concentration levels from low to near maximum packing as 15, 25 and 35 wt%. Examining the rheological behavior of the shear thickening fluid indicates that the increase of shear thickening fluid concentration leads to significant increase in the suspension’s initial, critical and ultimate (up to 104 Pa.s) viscosities, reduction of the critical shear rate, increase of viscoelastic modulus and instability of the suspension. The quasi-static puncture test results demonstrate with the increase of shear thickening fluid concentration, the maximum bearable load by the 15, 25 and 35 wt% shear thickening fluids-treated Twaron® composites increases by 132, 315 and 362%, and the energy absorption increases by 143, 159 and 209%, res...
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    33
    References
    18
    Citations
    NaN
    KQI
    []