Laser joining of glass to silicon using adhesive for MEMS packaging applications

2006 
Laser joining is a promising technique for wafer-level bonding. It avoids subjecting the complete MEMS package to a high temperature and/or the high electric field associated with conventional wafer-level bonding processes, using the laser to provide only localized heating. We demonstrate that a benzo-cyclo-butene (BCB) polymer, used as an intermediate bonding layer in packaging of MEMS devices, can be satisfactorily cured with a substantial reduction of curing time compared with an oven-based process by using laser heating. A glass-on-silicon cavity bonded with a BCB ring can be produced in few seconds at typical laser intensity of 1 W/mm2 resulting in a local temperature of ~ 300°C. Hermeticity and bond strength tests show that such cavities have similar or better performance than cavities sealed by a commercial substrate bonders which require a minimum curing time of 10 minutes. The influence of exposure time, laser power and pressure on degree of cure, bond strength and hermeticity is investigated. The concept of using a large area, uniform laser beam together with a simple mirror mask is tested, demonstrating that such a mask is capable of protecting the centre of the cavity from the laser beam; however to prevent lateral heating via conduction through the silicon a high conductivity heat sink is required to be in good thermal contact with the rear of the silicon.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    0
    Citations
    NaN
    KQI
    []