Growth stress and interdiffusion analysis of NiCoCrAlYTa coating during oxidation

2020 
The NiCoCrAlYTa coating deposited on Ni-based superalloy using arc ion plating (AIP) technology was subjected to isothermal oxidation in air at 1050°C for up to 200 h. The microstructure, oxides sc...