La-Faujasite zeolite activated with boron trifluoride: synthesis and application as solid acid catalyst for isobutane–isobutene alkylation

2021 
The sodium form of Faujasite Y (Na-FAU) zeolite has been synthesized by the hydrothermal method, and it has been exchanged with ammonium sulphate and later with lanthanum (III) chloride solutions to obtain the La-FAU catalyst. The three zeolites Na-FAU, NH4+-FAU and La-FAU have been characterized by microcrystalline X-ray diffraction, X-ray fluorescence, surface area, pore volume and Bronsted acid sites. The La-FAU catalyst has been successfully activated with boron trifluoride etherate, and it has been tested in the alkylation reaction of isobutane with isobutene up to 112 h of time on stream, since the raw La-FAU catalyst showed a rapid deactivation.