Shear bond strength of self-etching adhesive systems to Er:YAG-laser-prepared dentin

2009 
This study was conducted to compare the shear bond strengths of composite resin bonded to Er:YAG laser or bur-prepared dentin surfaces using three self-etching adhesive systems. The occlusal surfaces of 120 human third molars were ground flat to expose dentin. The dentin was prepared using either a carbide bur or an Er:YAG laser at 350 mJ/pulse and 10 Hz (fluence, 44.5 J/cm2). Three different self-etching adhesive systems were applied: iBond™, Xeno III™ and Clearfil SE Bond™. Rods of composite resin were bonded to dentin surfaces and shear bond tests were carried out. Both dentin surfaces after debonding and resin rods were observed using a scanning electron microscope. When the Xeno III™ was used, no difference was observed on shear bond strength values when bur and Er:YAG laser were compared. When using iBond™ and Clearfil SE Bond™, bond strength values measured on Er:YAG-laser-prepared surfaces were lower than those observed on bur-prepared surfaces. The absence of smear layer formation during the preparation of the dentin by the Er:YAG laser did not improve the adhesion values of self-etching adhesive systems.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    16
    References
    36
    Citations
    NaN
    KQI
    []