Thermoplastic molding the flame protected.

1996 
MASS THERMOPLASTIC MOLDING ARE fireproofing CONTAINING A) 40 to 98% by weight of a thermoplastic polyamide B) 1 to 40% by weight cyanurate MELANINA C) 1 to 50% by weight of a filler INORGANIC pin-shaped And pretreated with a silane compound, with an L / D ratio of 8: 1 to 35: 1 D) 0 to 30% by weight of other additives and processing aids giving percentages of components A) to D) 100%.