Liquefaction of ground tire rubber at low temperature

2018 
Abstract Low-temperature liquefaction has been investigated as a novel method for recycling ground tire rubber (GTR) into liquid using an environmentally benign process. The liquefaction was carried out at different temperatures (140, 160 and 180 °C) over variable time ranges (2–24 h) by blending the GTR with aromatic oil in a range from 0 to 100 parts per hundred rubber (phr). The liquefied GTR was separated into sol (the soluble fraction of rubber which can be extracted with toluene) and gel fractions (the solid fraction obtained after extraction) to evaluate the reclaiming efficiency. It was discovered that the percentage of the sol fraction increased with time, swelling ratio and temperature. Liquefied rubber was obtained with a high sol fraction (68.34 wt%) at 140 °C. Simultaneously, separation of nano-sized carbon black from the rubber networks occurred. The separation of carbon black from the network is the result of significant damage to the cross-linked-network that occurs throughout the liquefaction process. During liquefaction, a competitive reaction between main chain scission and cross-link bond breakage takes place.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    45
    References
    22
    Citations
    NaN
    KQI
    []