Descaling Behavior of 430 Hot-rolled Stainless Steel in HCl-based Solution

2016 
Descaling of hot-rolled stainless steel is generally implemented through pickling process in HNO3-HF mixed acids,which induces severe environmental concerns of nitrogen oxide(NOx)gases and nitrites.According to the electrochemical measurement,the mass loss test and the appearance analysis,a new pickling process which employed HCl-based solution was proposed and evaluated to provide theoretical basis for the development of environment-friendly and highly effective pickling process.Under the experimental condition,the HCl-based solution can compete with ordinary HNO3-HF mixed acids in terms of pickling efficiency,surface integrity and the removal of Crdepleted layer.The descaling process of 430hot-rolled stainless steel in the HCl-based solution consisted of three steps.The descaling solution penetrated the oxide scales into the underlying metal,dissolving the Cr-depleted layer and part of substrates.The oxide scales peeled off from the stainless steel and a polished and smooth surface was exposed.The descaled stainless steel was dissolved uniformly in the HCl-based solution;therefore,the pickling duration was vital for desired surface integrity.Under the static condition,the appropriate descaling time of 430 hotrolled stainless steel in HCl-based solution was 400 s.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    2
    Citations
    NaN
    KQI
    []