Functional Properties of Sm2NiMnO6Multiferroic Ceramics Prepared by Spark Plasma Sintering.

2015 
Sm2NiMnO6 is prepared by auto-combustion of a dried gel formed by heating a HNO3 solution of Sm(NO3)3, Ni(NO3)2, Mn, and citric acid (150 °C ignition temperature).