Composite fiberglass improved processability

2009 
reinforced fiber comprising (a) a heterophasic propylene copolymer (HECO), (b) a propylene homopolymer (H-PP1) and / or a propylene copolymer (C-PP1), and (c) fiber composition (F ), wherein (I) the propylene copolymer (C-PP1) comprises not more than 2.0% by weight of α-olefins of C2 to C10distintas propylene, (II) the propylene homopolymer (H-PP1) and the propylene copolymer (C-PP1) have an index of fusionMFR2 (230 ° C) measured according to ISO 1133 of at least 500 g / 10 min., and (III) the composition has a melt flow rate MFR2 (230 ° C ) measured according ISO 1133 of at least 10 g / 10min.