Contact sensitivity to nickel in white gold

1984 
Nickel release from white gold discs stored at room temperature for I week in synthetic sweat was analyzed. The nickel content of the discs was 2–15%. The nickel release from the discs was 0.09–0.82μg. Rhodium plating reduced the nickel release to 0.04–0.54 μg 18 nickel-sensitive women were patch tested with the while gold discs and all showed at least 1 positive patch test reaction. All the white gold discs gave a negative dimethylglyoxime test.