Photoluminescent properties of Eu3+-Eu2+ activated MAl2Si x O2x + 4 (M = Mg, Ca, Sr, Ba) phosphors prepared in air

2018 
: In this paper, MAl2 Six O2x+4 :Eu2+ /Eu3+ (Eu2+ + Eu3+ = 2%, molar ratio; M = Mg, Ca, Sr, Ba; x = 0, 0.5, 1, 1.5, 2) phosphors with different SiO2 concentrations (the ratio of SiO2 to MAl2 O4 is n%, n = 0, 50, 100, 150, 200, respectively) were prepared by high-temperature solid-state reaction under atmospheric air conditions. Their structures and photoluminescent properties were systematically researched. The results indicate that Eu3+ ions have been reduced and Eu2+ ions are obtained in air through the self-reduction mechanism. The alkaline earth metal ions and doping SiO2 strongly affect the crystalline phase and photoluminescent properties of samples, including microstructures, relative intensity of Eu2+ to Eu3+ , location of emission lines/bands. It is interesting and important that the emission color and intensities of europium-doped various phosphors which consist of aluminosilicate matrices prepared under atmospheric air conditions could be modulated by changing the kinds of alkaline earth metal and the content of SiO2 .
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    57
    References
    4
    Citations
    NaN
    KQI
    []