Wear of resin-modified glass ionomers: an in vitro study.

2001 
The purpose of this study was to evaluate the wear resistance and clinical applicability of resin-modified glass ionomer cements as restorative or fissure-sealing materials. The in vitro wear of resin-modified glass ionomers was compared to conventional glass ionomers, a resin-based sealant, and a composite resin. A three-body wear test (enamel block - polymethylmethacrylate powder - experimental dental material) was performed by 20,000 cycles with a load of 4kgf/cm2. The depth of wear of the experimental materials was measured and calculated using a computerized laser surface scanner. The glass ionomers generally showed more wear than the resin-based sealant and the composite resin, but there was no difference in wear between resin-modified and conventional glass ionomers. Type III ionomers (used for sealant) showed lower wear resistance than type II ionomers (used for restoration).
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    26
    References
    8
    Citations
    NaN
    KQI
    []