The invention provides an echelon releasing method for underground solid anticorrosion and antiscale agents, and the method comprises the following steps of step 1: charging imidazoline inhibitor with a dissolving speed of 0.12g/cm *h, imidazoline inhibitor with a dissolving speed of 0.01g/cm *h, organic phosphonate antiscale agent and clay or kaolin into a tablet press according to a proportion of 0.4: 1.6: 1: 2 to a prepare solid anticorrosion and antiscale agent 1; step 2: charging the imidazoline inhibitor with the dissolving speed of 0.12g/cm *h, the imidazoline inhibitor with the dissolving speed of 0.05g/cm *h, organic phosphonate antiscale agent and clay or kaolin into a tablet press according to a proportion of 0.4: 1.6: 1: 2 to prepare a solid anticorrosion and antiscale agent 2; selecting the solid anticorrosion and antiscale agent 1 when the underground temperature is more than 50DEG C, and selecting the solid anticorrosion and antiscale agent 2 when the underground temperature is less than 50DEG C; and directly charging the solid anticorrosion and antiscale agents before a tubular post is arranged or charging the solid anticorrosion and antiscale agent into a sieve tube, which is hung under a pump, to charge the solid anticorrosion and antiscale agent into an oil well.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    0
    Citations
    NaN
    KQI
    []