Tungstate Based Ceramics Obtained By Spark Plasma Sintering Method – Possible Material for Consolidation of Radioactive Wastes’ Components

2018 
The Spark Plasma Sintering method was used to produce high-density ceramics from tungstates SrWO 4 and NaNd(WO 4 ) 2 with scheelite structure. These compounds are proposed as possible matrices for the consolidation of radwaste components. Powder samples were obtained by coprecipitation method and studied by X-ray diffraction analysis (XRD) and scanning electron microscopy (SEM). After sintering, the samples retained their phase identity (scheelite structure). The total duration of sintering was ~ 13-15 min, the relative density was reached ~ 92, 99%.