Method and apparatus for producing silicon nitride or ferro silicon nitride by low pressure combustion

2002 
A process for preparing silicon (or ferrosilicon) nitride from silicon powder (or ferrosilicon) powder and the fine powder of silicon (or ferrosilicon) nitride as diluent by low-voltage combustion includes such steps as continuous burning at 900-1850 deg.C in vertical reacting furnace, cooling, and grinding.