Uji Kuat Tekan Paving Block Menggunakan Campuran Tanah dan Kapur Dengan Alat Pemadat Modifikasi

2016 
Paving blocks are widely used as a public building construction, especially for paving roads, yards, sidewalks, parking lots, etc. The use of materials such as paving block the main constituent of cement and sand is relatively expensive. So in this study will provide another alternative to using a mixture of soil and lime. Soil samples tested were from Kota Baru, South Lampung, with variations in the levels of the mixture used is 0%, 5%, 10%, 15%, and 20% and the curing time for 14 days, as well as with the treatment without burning and burning which will then be tested compressive strength and water absorption. The results showed that the compressive strength occurs at the most optimal mix of 15% and a decline in a mixture of 20%. The addition of lime percentage ≤15% resulted in the addition of compressive strength of paving blocks, while the addition of lime percentage of 20% resulted in a decrease in the compressive strength of the paving blocks. The compressive strength without burning still not meet the specifications of SNI 03-0691-1996, while paving blocks with burning the lime content of 15% is already included in the classification of the quality of D. Water absorption test values not meet the specifications of paving blocks SNI 03-0691-1996 which ranges from 3%-10%. Keywords : Paving block, kapur, kuat tekan, daya serap air
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    0
    Citations
    NaN
    KQI
    []