Method for preparing radioactive I ions

2013 
The invention discloses a method for preparing radioactive I ions. The preparation method comprises the following steps: a, taking aluminium oxide powder and tellurium dioxide powder in a mass ratio of 1:18-22, uniformly mixing the powder, and pressing the obtained mixture into a tellurium target with a thickness of 50-60 mg/cm ; b, placing the prepared tellurium target in a circular accelerator, and irradiating the tellurium target 2-3 h by Te (p, n) I, wherein the incident p particle beam intensity is 18-20 mu A, the energy is 18.5-20 MeV, and the angle of incidence is 6-10 DEG; meanwhile, cooling the tellurium target by using water in the process of irradiating, and after the irradiating is completed, placing the tellurium target to cool 4-6 h; c, placing the tellurium target in a quartz distillation tube of a destructive distillation device to distill, meanwhile, controlling the temperature to 750 DEG C so as to heat the tellurium target, so that radioactive I ions are escaped, and collecting the radioactive I ions. The problems that radionuclide I prepared in the prior art is low in yield and low in recovery rate are solved.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    1
    References
    0
    Citations
    NaN
    KQI
    []