Age hardening in (Ti1-xAlx)B2+Delta thin films

2017 
Thin films of (Ti0.71Al0.29)B2+1.08 have been deposited by magnetron sputtering. Post-deposition annealing at 1000 degrees C for 1 h results in increased hardness and elastic modulus, from 32 to 37 ...