생체모방형 비대칭 나노채널을 갖는 산화알루미늄 분리막 제조 및 이온 정류 특성
2020
In the present study, a biomimetic alumina membrane was fabricated by using selenic acid as an electrolyte to overcome the asymmetry limit of the square pulse anodization process. The prepared membrane has conical channels with a minimum diameter of 10 nm, a maximum diameter of 50 nm, and a length of 5 μm. The rectification property was higher than membranes fabricated by sulfuric acid. It showed 2.9 times larger current at +1 V than -1 V. Also, the membrane, which sulfonic acid group was introduced by surface modification, showed 4.2 times larger rectification property at -1 V than +1 V. Theoretical verifications were supported by the numerical analyses of 2D models. The results of the present study present a convenient method to fabricate two type membranes with different rectification properties and are expected to be used to control ion transport.