Poly(ethylene oxide) grafted to silicon surfaces : Grafting density and protein adsorption

1998 
Poly(ethylene oxide) (PEO) polymer, in linear and star form, was covalently grafted to silicon surfaces, and the surfaces were tested for their ability to adsorb proteins. Linear PEG of molecular weight 3400, 10 000, and 20 000 g/mol and star PEO molecules were coupled via their terminal hydroxyl groups activated by tresyl chloride to aminosilane-treated silicon wafers. The amount of PEO coupled to the surface was varied by changing the concentration of the tresyl-PEO solution. The dry PEO thickness on the surface was measured using X-ray photoelectron spectroscopy (XPS) and ellipsometry, from which the grafting density was calculated. The PEO surfaces were exposed to solutions of each of three proteins:  cytochrome-c, albumin, and fibronectin. The degree of adsorption of each protein was determined by XPS and ellipsometry and recorded as a function of PEO grafting density. All three proteins were found to reach zero adsorption at the highest grafting densities on all three PEG surfaces, which for all thr...
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    28
    References
    550
    Citations
    NaN
    KQI
    []