Electrochemical Machining—mechanisms of anodic dissolution

2016 
Abstract Electrochemical Machining (ECM) is widely used to produce products of high quality from metals and alloys. The work pieces are shaped by controlled anodic dissolution at extremely large current densities of about 100 A/cm 2 in neutral solutions (normally aqueous NaNO 3 ). Scaling down of the active area of the working electrode to 10 −3  cm 2 was necessary to enable current densities of some 100 A/cm 2 in a 3-electrode arrangement. Products were quantified at the electrolyte outlet by on-line photometry or fluorescence quenching and led to detailed models of the interface kinetics. The surface is described as a layered structure of an oxide film and a supersaturated, meta-stable viscous product film which is continuously removed by electrolyte flow. Fundamental dissolution mechanisms can be classified such as one-step or two-step anion makers, or spinel makers. Oxygen evolution reduces with increasing potential to about 10% of charge at >10 A/cm 2 .
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    33
    References
    56
    Citations
    NaN
    KQI
    []