Introduction Ceramic ball heads are well known in hip arthroplasty for their superior tribology performance and high burst strength. To assess the ball head performance and the in-vivo fracture risk Pandorf et al 2008 examined the burst strength of BIOLOX®forte (pure aluminium oxide ceramic, CeramTec GmbH, Plochingen, Germany) ball heads on clean standard test tapers and contaminated test tapers. They found that fat tissue and scratches are reducing the burst strength to 40% and to 20% of the reference burst strength, respectively. The aim of this work is to investigate if BIOLOX®delta (alumina matrix ceramic, CeramTec GmbH, Plochingen, Germany) ball heads show a similar behaviour as BIOLOX®forte ball heads with respect to taper contamination. Materials and Methods Each test series consisted of n=5 BIOLOX®delta 28–12/14 L ball heads and n=5 metal test tapers (Ti-6Al-4V, ISO 5832-3). For the reference series the metal tapers remained untouched representing the CeramTec standard test procedure. For the flui...
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    0
    Citations
    NaN
    KQI
    []