Structural, optical and electrical properties of zinc oxide thin films deposited by a spray pyrolysis technique

2015 
Zinc oxide(ZnO) thin films were deposited on glass substrates by spray pyrolysis technique decomposition of zinc acetate dihydrate in an ethanol solution with 30 m L of deposition rate, the ZnO thin films were deposited at two different temperatures: 300 and 350°C. The substrates were heated using the solar cells method.The substrate was R217102 glass, whose size was 30 17.5 1 mm3. The films exhibit a hexagonal wurtzite structure with a strong(002) preferred orientation. The higher value of crystallite size is attained for sprayed films at 350°C, which is probably due to an improvement of the crystallinity of the films at this point. The average transmittance of obtain films is about 90%–95%, as measured by a UV–vis analyzer. The band gap energy varies from 3.265 to 3.294 e V for the deposited Zn O thin film at 300 and 350°C, respectively. The electrical resistivity measured of our films are in the order 0.36 cm.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    6
    Citations
    NaN
    KQI
    []