The stress-strain hysteresis losses of Tb Dy Fe ( 0.30, 0.33, 0.40, 0.45, and 0.50) were measured at a variety of magnetic fields between 0 and 1600 Oe. Stress ranges from 0t o 10, 20, 40, and 60 MPa (the minus sign indicates compressive stresses) were used. The hysteresis loop area increased from 5.7 kJ m at to 10 kJ m at as the Tb concentration and the magnetic anisotropy increased. The position of the hysteresis loop shifted to larger compressive stresses as the magnetic field was increased allowing the strength of the damping to be controlled by the magnetic field. Index Terms—Hysteresis, magnetomechanical damping, Terfenol.