Methods of manufacturing fully annealed metal anodes are disclosed. The methods contemplate supplying metal and heating the metal until it has obtained a molten state. The molten metal is permitted to flow into a die and transported therethrough where it is cooled until it solidifies. The flow rate of the metal through the die and the extent of cooling are selected such that a fully annealed metal anode is obtained.