Influence of filler addition, storage medium and evaluation time on biaxial flexure strength and modulus of adhesive systems

2012 
Abstract Objective. This study evaluated the effects of filler addition, storage medium and time on biaxial flexural strength and flexural modulus of six adhesive systems. Materials and methods. The adhesives were either unfilled resins: Single Bond, PrimeB or filled resins: Single Bond Plus, Prime&Bond NT and One-Step Plus. Resin discs of each product (0.5 mm thick × 6.0 mm diameter) were prepared using silicon molds (n = 10). The discs were stored dry, in water, mineral oil or ethanol for 1 week or 3 months before biaxial flexural testing. Data were statistically analyzed by 3-way ANOVA and Tukey's post-hoc test (α = 0.05). The specimens were tested in a universal testing machine at 1.27 mm/min until failure occurred. Results. In general, the storage in ethanol led to significantly lower flexural strength and flexural modulus values than the other storage conditions for all adhesives in both storage periods. Filler addition increased flexural strength and flexural modulus for Prime...
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    38
    References
    17
    Citations
    NaN
    KQI
    []