Polypropylene composition containing a heterophasic propylene copolymer, comprising the heterophasic propylene copolymer of A) 60 to 75% by weight of a propylene homopolymer having a MFR of 8 to 60 g / 10 min (2, 16 kg / 230 ° C), B) between 25 and 40% by weight of an ethylene-propylene, wherein the heterophasic propylene copolymer containing XCS of between 22 and 33% by weight, whereby the XCS content has an ethylene content of between 45 and 65% by weight and whereby the XCS content having an intrinsic viscosity IV of 1.0 to 1.5 dl / g, wherein the polypropylene composition one MFRAB of between 10 and 35 g / 10 min, and whereby the polypropylene composition is free from filler.