Acute Posttraumatic Catastrophic Failure of a Second-generation, Highly Cross-linked Ultra-high-molecular-weight Polyethylene Patellar Component

2012 
Full article available online at Healio.com/Orthopedics. Search: 20120621-35 A 74-year-old man underwent total knee arthroplasty in 1996 and subsequent revision total knee arthroplasty for aseptic loosening in 2005. During revision, an all-polyethylene, 7-mm, second-generation, highly cross-linked ultra-high-molecular-weight polyethylene patellar component (Durasul; Zimmer, Warsaw, Indiana) was used. The patient recovered well, but he presented with severe acute pain after a popping feeling was detected during a game of golf in postoperative year 4. Radiographs demonstrated a fracture of the patellar component. At re-revision surgery, polyethylene fragments were encountered without visual evidence of wear. Appropriate rotational and axial alignment of the components was confirmed. Patellar revision was performed.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    11
    References
    10
    Citations
    NaN
    KQI
    []